Łunarska, Ellina (supervisor)
Institute of Physical Chemistry PAS
92 pp. : ill. ; 30 cm. ; Bibliogr. p. 86-92 ; Dissertations. Institute of Physical Chemistry PAS, 2004
application/pdf ; application/pdf
IChF PAN, sygn. B.368/04 ; click here to follow the link